Low temperature sintered ink for glass
Specially for the protection of plastic products processing water-based peeling protective oil, good construction, can be sprayed 40-80 microns at a time, cutting fluid resistance, polishing fluid resistance, wear resistance, scratch resistance, processing with high peeling strength, after adding by heating can quickly reduce the peeling strength of the coating.
General application method: spray
Spray -> IR baking 60-75 degrees,10-20 minutes -> CNC - > Polishing -> Heat automatic film removal
Paint film performance (PMMA material, PC material, UV surface)
Test item | Test method | Test result | |
Cutting fluid | Cutting fluid immersion | > The film can be removed normally after 30 minutes | |
Anti-polishing fluid | Polishing immersion | > The film can be removed normally after 30 minutes | |
Initial stripping force | Tensile machine | 200-400gf/25mm | |
Peeling force after heating | Bake at 120℃ for 2-3min | <10gf/mm |
Telephone: 0797-4216666 0752-3866668
Mail box: jxcicai@szcicai.cn
True transmission: 0797-4217188
Factory Address: Fine chemical Industry Park, Dingnan County, Ganzhou City, Jiangxi Province
R&d Center: No.23 Panli Road, Li Lin Town, Zhongkai High-tech Zone, Huizhou City, Guangdong Province